Do Moissanite Stones Get Cloudy? The Real Causes
Do moissanites get cloudy? Yes, and in almost every case the cloudiness is on the stone rather than in it. Moissanite is chemically stable and does not degrade with age, so a stone that looks hazy after a year is carrying a film on its pavilion and crown, not developing internal decay. The distinction matters because one problem is fixed with soapy water in ten minutes and the other would require replacing the stone.
The few cases where the haze really is inside the stone are narrow and specific, and they are worth knowing because no cleaning routine solves them. Below, the causes are separated by where the cloudiness sits, which is the only diagnostic that reliably points to the fix.

Why "cloudy" is almost always a film, not the stone
Moissanite is silicon carbide and it does not oxidise, hydrate or break down under normal wear. A stone that is a year old has the same crystal structure it had when it was cut. Nothing inside it is thickening or turning opaque, which is why an internal cause for haze is the rarest of the five and a surface cause is the usual one.
What does change is the surface. Skin oil, hand cream, hair product and soap residue collect on the pavilion, which is the underside of the stone, where they are protected from the cloth that polishes the top and invisible from above. That film scatters light instead of transmitting it, and the stone reads as dull, grey or cloudy while the top facet still sparkles under a direct lamp. This is the single most common cause, and it is covered in more detail in moissanite clouding versus dirt.
Five real causes, and how each one looks
| Cause | Where the haze sits | What it looks like | Fixable at home |
|---|---|---|---|
| Oil and product film | Pavilion, girdle, under prongs | Dull grey from above, bright under direct light | Yes, with soap and a brush |
| Hard water and soap scum | Girdle and lower facets, chalky edge | White ring around the stone's edge | Yes, with distilled water rinse |
| Prong and setting abrasion | Facet junctions where metal rubs | Fine scratches, scattered light at edges | No, needs a lapidary repolish |
| Coating or treatment film | Uniform over the crown | Even haze with no clear patches | Sometimes, by the original supplier |
| Internal inclusions at high magnification | Inside the stone, pinpoint | Visible only at 10x, no effect face-up | Not a defect |
The first two rows account for nearly all complaints. The fourth needs a word: some moissanite is sold with a surface coating intended to change colour or increase brilliance, and a coating that degrades produces an even, all-over haze that cleaning will not touch. If the haze is uniform across the crown and the pavilion is clean, suspect the surface rather than the stone.
The prong row deserves its own explanation, because it is the one cause a buyer can spot and a jeweller has to fix. Where a prong contacts the crown, metal and stone touch across a very small area under real pressure. Over years that contact polishes and then scratches the facet beneath, and the damaged patch scatters light like a smudge that will not come off. It appears first at the junction, where brushes cannot reach, so it is mistaken for stubborn dirt.

Cleaning it properly, in the right order
Warm water, a drop of mild dish soap, and a soft brush. Work the brush against the pavilion and around each prong, because that is where the film accumulates. Rinse in warm water, then in distilled water if your tap supply is hard, and dry with a lint-free cloth rather than letting it air dry, since air drying leaves mineral spots.
Do this weekly for a ring worn daily. The common failure is doing it monthly and concluding the stone is cloudy when it is simply dirty, then escalating to a jeweller for a problem that a brush would have solved. The full method, including what not to use, is in how to clean moissanite.
Two things to avoid. Ultrasonic cleaning is safe for moissanite itself but can loosen stones in a setting that was not tightened properly, and it damages some colored stones set alongside it. Steam is fine on the stone and hard on certain treatments. Both are worth checking against the whole piece rather than against the centre stone alone; ultrasonic cleaning by stone type sets out which combinations are safe.
There is also a difference between a closed-back setting and an open one. A bezel that sits flat against the finger traps moisture and product between the stone and the metal, and the film builds faster there than in a prong setting where water flows through. If a bezelled stone clouds within days of every cleaning, the answer is more frequent cleaning, not a different cleaner. Bezel versus prong setting covers how the two trap debris differently.
The hardness question, and why it is not the problem
Moissanite is hard enough that ordinary wear does not scratch it, and hard enough that it will scratch most other jewelry it is stored against. It is not hard enough to be immune to everything, and the two things that do mark it are worth knowing.
Diamond abrasives, including the grit in some polishing cloths and in diamond-studded tools, will scratch moissanite because diamond is harder than silicon carbide. And moissanite against moissanite in a jewelry box will produce fine wear over years, because two stones of equal hardness abrade each other. Neither is a cloudiness mechanism in the ordinary sense; both produce surface scratches that scatter light at the facet edges.
The practical rule is to store moissanite separately, in its own compartment or pouch, and never to polish it with a cloth marketed for diamond. Both habits remove the two mechanisms that actually damage the surface.
What the setting metal contributes
The metal around the stone is the second source of haze, and the density of that metal tells you how much material is available to deposit. Sterling silver is the metal most often implicated, because it tarnishes and the tarnish film migrates onto the pavilion where a cloth cannot reach it.
| Metal in the setting | Density (g/cm³) | Does it deposit film on the stone | What removes it |
|---|---|---|---|
| S925 sterling silver | 10.36 | Yes, tarnish film on the pavilion | Silver-dip on the metal only, never on the stone, then a distilled water rinse |
| 14K gold | 13.5 | Rarely, only from soap trapped under prongs | Warm water, mild soap, soft brush |
| 18K gold | 15.5 | Rarely, same as 14K | Warm water, mild soap, soft brush |
| PT950 platinum | 20.7 | No film, but the metal itself smears onto facet edges under impact | Bench polish by a jeweller |
Read the table as a ranking, not a promise. A silver setting with a closed back is the worst combination, because tarnish forms where air is trapped and no brush reaches. An open-back silver setting dries faster and hazes more slowly. Silver accounts for 471 of the 708 styles on this site, which is why silver is the metal most buyers are asking about when they report a cloudy stone.
What is genuinely inside the stone
Moissanite is grown, and grown crystals can carry inclusions: tiny needles, pinpoints or growth patterns. These are normal, they are assessed under magnification, and they do not cause haze visible to the eye. A stone graded VVS1 has inclusions that are very difficult to find even at ten times magnification, which is the practical meaning of the grade covered in what VVS1 means for moissanite.
What does affect face-up appearance is not inclusions but cut. A stone with a shallow pavilion or a large table can leak light through the bottom instead of returning it, and the result reads as a dull, glassy centre that no cleaning will fix. That is a cutting problem, visible from the moment of purchase, and it is the one defect most often mistaken for cloudiness in a photograph.
Double refraction and the "hazy" look people describe
Moissanite is doubly refractive, which means light entering it splits into two paths. The visible effect is a slight doubling of facet edges when you look closely, and a distinctive softness in the stone's internal appearance compared with diamond. That is a property of the material, present from day one, and it does not increase with age.
Buyers who describe a stone as hazy often mean this. The test is simple: compare the stone to a photograph of it taken when new. If the character is identical, nothing has changed and the stone is behaving as moissanite does. If the character has genuinely worsened, the cause is on the surface. The physics behind the effect is explained in moissanite double refraction.
Tarnish on the setting reads as cloudiness on the stone
Silver tarnishes, and tarnish on the setting around a stone produces a dark halo that makes the stone look duller than it is. This is not the stone failing. It is the metal reflecting less light back through the pavilion, plus the visual contrast of a dark rim against a bright facet.
Silver is the dominant material here at 471 of 708 styles, so a moissanite in sterling silver is the most common configuration a buyer will encounter, and the one where setting tarnish most often gets blamed on the stone. Cleaning the metal and the stone together solves it. Does 925 silver tarnish covers how fast this happens.
When cleaning stops working
If a stone stays hazy after two proper cleanings a week apart, with the brush worked against the pavilion both times, then the cause is not film and cleaning will not fix it. At that point there are three possibilities: surface scratches from abrasion, a degraded coating, or a cutting problem that was always there.
Scratches can be repolished by a lapidary, though the cost has to be weighed against the stone's value. A coating has to be dealt with by the supplier that applied it. A cutting problem is not repairable at all, and the honest answer is that the stone was always like that and the earlier photographs will show it.
What is worth saying plainly: none of those three is a normal outcome of ownership. Moissanite does not cloud with age. If a piece is hazy and the film has been ruled out, the cause was either present at purchase or introduced by handling, and no amount of time will make it worse on its own.
A short routine that prevents the complaint
- Clean weekly with warm water, mild soap and a soft brush, working the pavilion.
- Rinse with distilled water if the local supply is hard, and dry with a lint-free cloth.
- Store the piece in its own pouch or compartment, away from other stones.
- Remove it before swimming, cleaning, and any contact with chlorine.
- Apply cosmetics and hair product before putting the piece on, not after.
- Check the prongs twice a year; a loose stone traps film and can chip at the girdle.
That list is unglamorous and it is the whole answer. The pieces that stay bright are the ones that get brushed, not the ones that get bought at a higher grade. A VVS1 stone with a filthy pavilion looks worse than a lower grade that is cleaned, and the difference is entirely in the routine.